{"id":1037,"date":"2013-10-05T16:15:51","date_gmt":"2013-10-05T16:15:51","guid":{"rendered":"http:\/\/nanovea.com\/?p=1037"},"modified":"2015-06-17T16:14:45","modified_gmt":"2015-06-17T16:14:45","slug":"makrokratzprufung-von-eloxalschichten","status":"publish","type":"post","link":"https:\/\/nanovea.com\/de\/macro-scratch-testing-of-anodized-coatings\/","title":{"rendered":"Eloxierte Beschichtungen Makro-Kratztest"},"content":{"rendered":"<p>Der Prozess des Kratzens wird auf kontrollierte und \u00fcberwachte Weise simuliert, um adh\u00e4sive oder koh\u00e4sive Ausf\u00e4lle zu beobachten. Bei dieser Anwendung wird der Nanovea Mechanical Tester in seiner Makroversion <a title=\"Kratzertest\" href=\"https:\/\/nanovea.com\/micro-scratch-tester\" target=\"_blank\">Kratzertest<\/a> Modus wird verwendet, um die Belastung zu messen, die erforderlich ist, um ein Versagen von Eloxalschichten zu verursachen, die mit verschiedenen Verfahren hergestellt wurden.<\/p>\n<p><a href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/macro-scratch-anodized.pdf\">Makrokratzpr\u00fcfung von anodisierten Beschichtungen<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>The process of scratching is simulated in a controlled and monitored manner to observe adhesive or cohesive failures. In this application, the Nanovea Mechanical Tester in its macro scratch testing mode is used to measure the load required to cause failure to anodized coatings produced by different processes. Macro Scratch Testing of Anodized Coatings<\/p>","protected":false},"author":1,"featured_media":1038,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[149],"class_list":["post-1037","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-anodized-coatings"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts\/1037","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/comments?post=1037"}],"version-history":[{"count":3,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts\/1037\/revisions"}],"predecessor-version":[{"id":1730,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts\/1037\/revisions\/1730"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/media\/1038"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/media?parent=1037"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/categories?post=1037"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/tags?post=1037"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}