Category: Hardness vs Depth

Hardness Distribution of Hardened Metal Using Nanoindentation
In this application, the Nanovea Mechanical Tester in nanoindentation mode is used to measure the
hardness distribution of the hardened surface on the cross section of a surface hardened metal.
Hardness Distribution of Hardened Metal Using Nanoindentation