{"id":967,"date":"2014-03-05T13:43:50","date_gmt":"2014-03-05T13:43:50","guid":{"rendered":"http:\/\/nanovea.com\/?p=967"},"modified":"2015-06-16T21:16:12","modified_gmt":"2015-06-16T21:16:12","slug":"%d9%82%d9%8a%d8%a7%d8%b3-%d9%83%d9%81%d8%a7%d9%81-%d9%85%d8%af%d8%a7%d8%b3-%d8%a7%d9%84%d9%85%d8%b7%d8%a7%d8%b7-%d8%a8%d8%a7%d8%b3%d8%aa%d8%ae%d8%af%d8%a7%d9%85-%d9%82%d9%8a%d8%a7%d8%b3-%d8%a7%d9%84","status":"publish","type":"post","link":"https:\/\/nanovea.com\/ar\/contour-measurement-of-rubber-tread-using-3d-profilometry\/","title":{"rendered":"\u0642\u064a\u0627\u0633 \u0645\u062d\u064a\u0637 \u0627\u0644\u0645\u062f\u0627\u0633 \u0627\u0644\u0645\u0637\u0627\u0637\u064a \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0645\u0642\u064a\u0627\u0633 \u0627\u0644\u0645\u0644\u0627\u0645\u062d \u062b\u0644\u0627\u062b\u064a \u0627\u0644\u0623\u0628\u0639\u0627\u062f"},"content":{"rendered":"<p>\u0641\u064a \u0647\u0630\u0627 \u0627\u0644\u062a\u0637\u0628\u064a\u0642 \u0646\u0627\u0646\u0648\u0641\u064a\u0627 ST400 <a title=\"\u0645\u0642\u064a\u0627\u0633 \u0628\u0631\u0648\u0641\u064a\u0644\u0648\u0645\u062a\u0631\" href=\"https:\/\/nanovea\/profilometers\" target=\"_blank\">\u0645\u0642\u064a\u0627\u0633 \u0627\u0644\u0645\u0644\u0627\u0645\u062d<\/a> \u064a\u0633\u062a\u062e\u062f\u0645 \u0644\u0642\u064a\u0627\u0633 \u0633\u0637\u062d \u0648\u0637\u0631\u0642 \u0627\u0644\u0625\u0637\u0627\u0631\u0627\u062a \u0627\u0644\u0645\u0637\u0627\u0637\u064a\u0629. \u062a\u0645 \u0627\u062e\u062a\u064a\u0627\u0631 \u0645\u0633\u0627\u062d\u0629 \u0627\u0644\u0633\u0637\u062d \u0627\u0644\u062a\u064a \u062a\u0645 \u0642\u064a\u0627\u0633\u0647\u0627 \u0628\u0634\u0643\u0644 \u0639\u0634\u0648\u0627\u0626\u064a \u060c \u0648\u0643\u0627\u0646\u062a \u0643\u0628\u064a\u0631\u0629 \u0628\u0645\u0627 \u064a\u0643\u0641\u064a \u0628\u062d\u064a\u062b \u064a\u0645\u0643\u0646 \u0627\u0633\u062a\u0642\u0631\u0627\u0621\u0647\u0627 \u0644\u0639\u0645\u0644 \u0627\u0641\u062a\u0631\u0627\u0636\u0627\u062a \u062d\u0648\u0644 \u0633\u0637\u062d \u0623\u0643\u0628\u0631 \u0628\u0643\u062b\u064a\u0631. \u0633\u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0623\u0628\u0639\u0627\u062f \u0627\u0644\u0643\u0646\u062a\u0648\u0631 \u0648\u0627\u0644\u0639\u0645\u0642 \u0648\u062e\u0634\u0648\u0646\u0629 \u0627\u0644\u0633\u0637\u062d \u0648\u0627\u0644\u0645\u0633\u0627\u062d\u0629 \u0627\u0644\u0645\u062a\u0637\u0648\u0631\u0629 \u0647\u0646\u0627 \u0644\u062a\u062d\u062f\u064a\u062f \u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u0637\u0627\u0637.<\/p>\n<p><a href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/contour-measurement.pdf\">\u0642\u064a\u0627\u0633 \u0645\u062d\u064a\u0637 \u0627\u0644\u0645\u062f\u0627\u0633 \u0627\u0644\u0645\u0637\u0627\u0637\u064a \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0645\u0642\u064a\u0627\u0633 \u0627\u0644\u0645\u0644\u0627\u0645\u062d \u062b\u0644\u0627\u062b\u064a \u0627\u0644\u0623\u0628\u0639\u0627\u062f<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>In this application the Nanovea ST400 Profilometer is used to measure the surface and treads of a rubber tire. The surface area measured was selected at random, and was large enough that it could be extrapolated to make assumptions about a much larger surface. Contour dimensions, depth, surface roughness, and developed area will be used [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":968,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[136],"class_list":["post-967","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-rubber-tread"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/posts\/967","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/comments?post=967"}],"version-history":[{"count":4,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/posts\/967\/revisions"}],"predecessor-version":[{"id":11386,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/posts\/967\/revisions\/11386"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/media\/968"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/media?parent=967"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/categories?post=967"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/tags?post=967"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}