{"id":864,"date":"2014-11-05T04:24:16","date_gmt":"2014-11-05T04:24:16","guid":{"rendered":"http:\/\/nanovea.com\/?p=864"},"modified":"2015-06-08T21:36:06","modified_gmt":"2015-06-08T21:36:06","slug":"steel-surface-characterization-using-3d-profilometry","status":"publish","type":"post","link":"https:\/\/nanovea.com\/ar\/steel-surface-characterization-using-3d-profilometry\/","title":{"rendered":"\u062a\u0648\u0635\u064a\u0641 \u0633\u0637\u062d \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0642\u064a\u0627\u0633\u0627\u062a \u0627\u0644\u0645\u0644\u0641 \u0627\u0644\u0634\u062e\u0635\u064a \u062b\u0644\u0627\u062b\u064a\u0629 \u0627\u0644\u0623\u0628\u0639\u0627\u062f"},"content":{"rendered":"<p>\u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0643\u0627\u0645\u064a\u0631\u0627 \u0641\u064a \u0627\u0644\u0628\u062f\u0627\u064a\u0629 \u0644\u062e\u064a\u0627\u0637\u0629 \u0645\u0633\u0627\u062d\u0629 \u0635\u0648\u0631\u0629\u060c 6 \u0645\u0645 2\u060c \u062b\u0645 \u062a\u062d\u062f\u064a\u062f \u0645\u0646\u0637\u0642\u0629 \u0627\u0644\u0627\u0647\u062a\u0645\u0627\u0645 \u0628\u0635\u0631\u064a\u064b\u0627\u060c 2 \u0645\u0645 2\u060c \u0644\u0644\u0642\u064a\u0627\u0633. \u0646\u0627\u0646\u0648\u0641\u064a\u0627 ST400 <a title=\"\u0645\u0642\u064a\u0627\u0633 \u0628\u0631\u0648\u0641\u064a\u0644\u0648\u0645\u062a\u0631\" href=\"https:\/\/nanovea.com\/profilometers\" target=\"_blank\">\u0645\u0642\u064a\u0627\u0633 \u0627\u0644\u0645\u0644\u0627\u0645\u062d<\/a> \u062b\u0645 \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0647\u0627 \u0644\u0625\u0646\u0634\u0627\u0621 \u062e\u0631\u064a\u0637\u0629 \u0627\u0631\u062a\u0641\u0627\u0639 \u0644\u0644\u0633\u0637\u062d \u0648\u062a\u0645\u062a \u062f\u0631\u0627\u0633\u0629 \u0627\u0644\u062e\u0634\u0648\u0646\u0629 \u0648\u0627\u0644\u0646\u0642\u0631.<\/p>\n<p><a title=\"\u062a\u0648\u0635\u064a\u0641 \u0627\u0644\u0633\u0637\u062d\" href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/steel-surface-characterization.pdf\" target=\"_blank\">\u062a\u0648\u0635\u064a\u0641 \u0633\u0637\u062d \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0642\u064a\u0627\u0633\u0627\u062a \u0627\u0644\u0645\u0644\u0641 \u0627\u0644\u0634\u062e\u0635\u064a \u062b\u0644\u0627\u062b\u064a\u0629 \u0627\u0644\u0623\u0628\u0639\u0627\u062f<\/a><a href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/steel-surface-characterization.pdf\"><br \/>\n<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>The camera is used initially to stitch an image area, 6mm2, and then visually select an area of interest, 2mm2, for measurement. The Nanovea ST400 Profilometer is then used to create a height map of the surface and the roughness and pitting were studied. Steel Surface Characterization Using 3D Profilometry<\/p>","protected":false},"author":1,"featured_media":865,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[55],"class_list":["post-864","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-surface-characterization"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/posts\/864","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/comments?post=864"}],"version-history":[{"count":4,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/posts\/864\/revisions"}],"predecessor-version":[{"id":11383,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/posts\/864\/revisions\/11383"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/media\/865"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/media?parent=864"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/categories?post=864"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/tags?post=864"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}