{"id":1066,"date":"2013-08-06T18:29:12","date_gmt":"2013-08-06T18:29:12","guid":{"rendered":"http:\/\/nanovea.com\/?p=1066"},"modified":"2015-06-17T17:00:55","modified_gmt":"2015-06-17T17:00:55","slug":"carbon-fiber-surface-measurement-using-3d-profilometry","status":"publish","type":"post","link":"https:\/\/nanovea.com\/ar\/carbon-fiber-surface-measurement-using-3d-profilometry\/","title":{"rendered":"\u0642\u064a\u0627\u0633 \u0627\u0644\u0633\u0637\u062d \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0645\u0642\u064a\u0627\u0633 \u0627\u0644\u0645\u0644\u0627\u0645\u062d \u062b\u0644\u0627\u062b\u064a \u0627\u0644\u0623\u0628\u0639\u0627\u062f"},"content":{"rendered":"<p>\u0641\u064a \u0647\u0630\u0627 \u0627\u0644\u062a\u0637\u0628\u064a\u0642 \u0646\u0627\u0646\u0648\u0641\u064a\u0627 ST400 <a title=\"\u0645\u0642\u064a\u0627\u0633 \u0628\u0631\u0648\u0641\u064a\u0644\u0648\u0645\u062a\u0631\" href=\"https:\/\/nanovea.com\/profilometers\" target=\"_blank\">\u0645\u0644\u0641 \u0627\u0644\u062a\u0639\u0631\u064a\u0641<\/a>r \u064a\u0633\u062a\u062e\u062f\u0645 \u0644\u0642\u064a\u0627\u0633 \u0633\u0637\u062d \u0642\u0637\u0639\u0629 \u0645\u0643\u0634\u0648\u0641\u0629 \u0645\u0646 \u0623\u0644\u064a\u0627\u0641 \u0627\u0644\u0643\u0631\u0628\u0648\u0646. \u062a\u0645 \u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u0645\u0646\u0637\u0642\u0629 \u0627\u0644\u062a\u064a \u062a\u0645 \u0642\u064a\u0627\u0633\u0647\u0627 \u0628\u0634\u0643\u0644 \u0639\u0634\u0648\u0627\u0626\u064a \u060c \u0648\u0627\u0641\u062a\u0631\u0636 \u0623\u0646\u0647\u0627 \u0643\u0628\u064a\u0631\u0629 \u0628\u0645\u0627 \u064a\u0643\u0641\u064a \u0628\u062d\u064a\u062b \u064a\u0645\u0643\u0646 \u0627\u0633\u062a\u0642\u0631\u0627\u0621\u0647\u0627 \u0644\u0639\u0645\u0644 \u0627\u0641\u062a\u0631\u0627\u0636\u0627\u062a \u062d\u0648\u0644<br \/>\n\u0633\u0637\u062d \u0623\u0643\u0628\u0631 \u0628\u0643\u062b\u064a\u0631. \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u062e\u0634\u0648\u0646\u0629 \u0627\u0644\u0633\u0637\u062d \u060c \u0648\u0645\u0633\u0627\u062d\u0629 \u0627\u0644\u0633\u0637\u062d \u060c \u0648\u0627\u0644\u0637\u0648\u0644 \u0627\u0644\u0645\u0648\u062c\u064a \u060c \u0648\u0627\u0644\u062a\u062d\u0644\u064a\u0644 \u0627\u0644\u0646\u0645\u0637\u064a \u0647\u0646\u062f\u0633\u064a \u0645\u062a\u0643\u0631\u0631 \u0648\u0645\u0639\u0644\u0645\u0627\u062a \u0627\u0644\u0633\u0637\u062d \u0627\u0644\u0623\u062e\u0631\u0649 \u0644\u062a\u0648\u0635\u064a\u0641 \u0627\u0644\u0633\u0637\u062d.<\/p>\n<p><a href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/carbon-fiber-measurement.pdf\">\u0642\u064a\u0627\u0633 \u0627\u0644\u0633\u0637\u062d \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0645\u0642\u064a\u0627\u0633 \u0627\u0644\u0645\u0644\u0627\u0645\u062d \u062b\u0644\u0627\u062b\u064a \u0627\u0644\u0623\u0628\u0639\u0627\u062f<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>In this application the Nanovea ST400 Profilometer is used for surface measurement of an exposed piece of carbon fiber. The area measured was selected at random, and assumed large enough in that it could be extrapolated to make assumptions about a much larger surface. Surface roughness, surface area, wavelength, fractal analysis and other surface parameters [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":1067,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[155],"class_list":["post-1066","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-surface-measurement"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/posts\/1066","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/comments?post=1066"}],"version-history":[{"count":3,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/posts\/1066\/revisions"}],"predecessor-version":[{"id":1741,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/posts\/1066\/revisions\/1741"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/media\/1067"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/media?parent=1066"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/categories?post=1066"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/tags?post=1066"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}