{"id":26301,"date":"2026-03-25T20:22:07","date_gmt":"2026-03-25T20:22:07","guid":{"rendered":"https:\/\/nanovea.com\/wp-content\/uploads\/2026\/03\/stent-groove-coating-high-adhesion-sample4-nano-scratch-173mn.jpg"},"modified":"2026-03-25T20:22:25","modified_gmt":"2026-03-25T20:22:25","slug":"stent-groove-coating-high-adhesion-sample4-nano-scratch-173mn","status":"inherit","type":"attachment","link":"https:\/\/nanovea.com\/ar\/stent-coating-adhesion-testing-nano-scratch\/stent-groove-coating-high-adhesion-sample4-nano-scratch-173mn\/","title":{"rendered":"Nano Scratch Track Showing Higher Adhesion in Groove \u2013 Sample 4"},"author":7,"featured_media":0,"comment_status":"open","ping_status":"closed","template":"","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0},"attachment_category":[],"attachment_tag":[],"class_list":["post-26301","attachment","type-attachment","status-inherit","hentry"],"description":{"rendered":"<p class=\"attachment\"><a href='https:\/\/nanovea.com\/wp-content\/uploads\/2026\/03\/stent-groove-coating-high-adhesion-sample4-nano-scratch-173mn.jpg'><img decoding=\"async\" width=\"300\" height=\"162\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2026\/03\/stent-groove-coating-high-adhesion-sample4-nano-scratch-173mn.jpg\" class=\"attachment-medium size-medium\" alt=\"stent groove coating adhesion sample 4 nano scratch 173 mN minimal failure testing\" \/><\/a><\/p>\n<p>Nano scratch track inside a stent groove showing improved coating adhesion and delayed failure at Lc \u2248 173 mN under the same testing conditions.<\/p>\n"},"caption":{"rendered":"<p>Nano scratch track inside a stent groove showing improved coating adhesion and delayed failure at Lc \u2248 173 mN under the same testing conditions.<\/p>\n"},"alt_text":"stent groove coating adhesion sample 4 nano scratch 173 mN minimal failure testing","media_type":"image","mime_type":"image\/jpeg","media_details":{"width":1794,"height":966,"file":"2026\/03\/stent-groove-coating-high-adhesion-sample4-nano-scratch-173mn.jpg","filesize":65977,"sizes":{},"image_meta":{"aperture":"0","credit":"","camera":"","caption":"","created_timestamp":"0","copyright":"","focal_length":"0","iso":"0","shutter_speed":"0","title":"","orientation":"0","keywords":[]}},"post":26271,"source_url":"https:\/\/nanovea.com\/wp-content\/uploads\/2026\/03\/stent-groove-coating-high-adhesion-sample4-nano-scratch-173mn.jpg","_links":{"self":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/media\/26301","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/media"}],"about":[{"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/types\/attachment"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/users\/7"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/comments?post=26301"}],"wp:term":[{"taxonomy":"attachment_category","embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/attachment_category?post=26301"},{"taxonomy":"attachment_tag","embeddable":true,"href":"https:\/\/nanovea.com\/ar\/wp-json\/wp\/v2\/attachment_tag?post=26301"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}