Honeycomb Panel Finish, Tribology and Mechanical Properties
Honeycomb panel analysis including mechanical properties using microindentation, surface finish using 3D profilometery and wear resistance using Tribometer.
MECHANICAL: https://nanovea.com/App-Notes/honeycomb-mechanical-behavior.pdf
PROFILOMETRY: https://nanovea.com/App-Notes/honeycomb-panel-finish.pdf
TRIBOLOGY: https://nanovea.com/App-Notes/honeycomb-panel-wear-resistance.pdf