MECHANICAL TESTERS SOFTWARE INTRO
|
 |
Indentation Software
The powerful indentation software offers ASTM E2546 and also Martens method of analysis. User-friendly software with real-time display of depth versus load curves and calculation of hardness & elastic modulus. Automatic data averaging. Holding the maximum load or depth constant over time for Creep data. Easily save Images from color camera (save as part of file or separate JPEG for export). Full range of calculation including indentation, plastic work, flow stress, plastic & elastic energy. Automated multi-sample handling. Mapping and positioning of each indent with microscope. Precise relocation of each indent. Data export in ASCII format. Latest Windows OS software and User-friendly w/ free software updates. Sinus mode analysis (DMA) for viscoelastic properties. Creep data plotted separately on depth versus time graph. Multi cycle with increasing depth for hardness and elastic modulus versus depth. Multi-cycle constant load for fatigue test. Automatic report for easy printing User Channel (optional).
|
 |
Scratch Software
The Nanovea Scratch Tester Software is a complete software package for controlling test parameters such as: speed, loading rate and scratch length, as well as analyzing test results. Full panoramic view with easy determination of critical loads with associated photo of failures. Real time display of Acoustic Emission, Depth, Frictional Force versus Load / Displacement. Images incorporated directly into the scratch file for easy reference. On-line correlation between measured data and optical observation. Pre and post profile scan for the study of plastic and elastic deformation. Advanced Panoramic view of the full scratch with direct visual correlation to depth, load, friction and acoustic emission data versus displacement curve. Associated load automatically indicated on the picture for easy identification. Multi-pass scratch testing for the characterization of the wear properties of the coating. Constant and progressive loads. Control of all the parameters: Speed, loading rate, and scratch length. Zoom Functions. Data export in ASCII format Latest Windows OS software and user-friendly with free software updates.Automatic report for easy printing User Channel (optional)
|
 |
Wear | Friction Software
The Wear & Friction Software includes a complete set of features for installation of analyzing wear and friction data. Real-time display of Coefficient of friction and depth. Wear rate calculation of ball and disk. Data export in CSV format for Excel. Data filtering. Graph manipulations. Test parameters & information editing. Note saving.
|
 |
3D Mechanical Software
The 3D Mechanical Software is a complete software package for scanning using the integrated non-contact profiling sensor. User friendly ability to scan specified areas of interest or a single profile. Creates 3D representation of the scan. Quick analysis of roughness, critical dimensions, topography and full pre and post test area profile. Zoom Functions. Data export in ASCII format & Mountain analysis software. Analyze surface distance and height. Allows user to compare scan with optical microscope observation. |
 |
Nanovea PRVision Software
PRVision can be included in Mechanical Software when an optional camera is included. PRVision was designed to automatically recognize features from a user-trained image file. The surface is scanned while automatically recognizing all features of interest; then either automatically indents every feature found or a selectively chosen by the user. PRVision can also be used to reference sample orientation during a Macro measurement, which will automatically correct for rotations or displacement created when samples are loaded and unloaded from their holder. This option will significantly reduce setup time when a surface pattern or if several samples will be measured. Ideal for using hardness as a quality control measure.
|